December 15, 2017
A subsidiary of PV equipment supplier Amtech Systems has received a follow-on order for three next generation solar Atomic Layer Deposition (ALD) systems.
October 18, 2017
DK Electronic Materials Inc. (DKEM) has launched a new generation of front-side metallization paste. ‘DK92’ series front-side metallization pastes have been developed to be compatible with different passivation technologies and processes for PERC solar cells, including ALD (spatial ALD, and time-based dual-side passivated ALD), PECVD (remote plasma and direct plasma) as well as other non-AlOx passivation solutions to boost the diversified PERC technologies and to further lower the LCOE.